Implantable and neural devices

Wafer-Level Fabrication
for Implantable Devices

Fabrication steps for implantable and neural interface devices: thin-film metal on polyimide, UBM and fluxless AuSn pads for chip attach on flexible substrates, through-glass vias for feedthrough designs, electrode arrays and glass bonding. Each step is set up on test wafers carrying your own polymer before your device wafers go in.

AuSn bump services →

Metal on polyimideAuSn on UBM padsLift-off patterningGlass through-viasElectrode arraysGlass bonding
80/20
AuSn
standard ratio
Test first
Each step tried on
your own polymer
Ti/Au · Pt
Electrode
metals
4 to 8 in
Carrier wafer
diameters
What we build

Thin-film interconnects for devices that bend, and glass parts for their packages

Implantable devices combine flexible polymer interconnects with rigid chips and sealed packages. We fabricate the thin-film metal, the chip-attach pads and the glass parts, with each wet step chosen for the polymer you use.

Chip, attached in your bonding reflowAuSn pad, shipped as depositedUBM in the polyimide openingPolyimide with metal routingCarrier wafer (glass or silicon)

Schematic, not to scale.

Thin-film metal on polyimide

Ti/Au, Ti/Pt/Au and multi-metal stacks patterned by lift-off on polyimide-coated wafers and on polyimide film carriers. See PI film fabrication.

UBM and AuSn pads for chip attach

Fluxless AuSn deposited as an Au/Sn multilayer on UBM pads over polyimide, patterned by lift-off and shipped as deposited, so the alloy forms in your bonding reflow. See AuSn bumps.

Daisy-chain bonding test wafers

AuSn and UBM on your daisy-chain wafers, or daisy-chain structures built to your layout, to qualify chip attach on a flexible stack before real chips are committed. See daisy-chain test dies.

Glass through-vias for feedthroughs

Through-glass vias in borosilicate and other glasses for feedthrough designs in glass packages. The via metal and the fill are reviewed against your design. See TGV fabrication.

Microelectrode arrays

Ti/Au or Pt electrodes with SU-8 or polyimide insulation and defined openings, on glass, silicon or polyimide. See neural interface microfabrication.

Glass bonding steps

Anodic glass-to-silicon bonding and patterned metal seal frames for cavities and lids. See anodic bonding.

At a glance

Wafer-Level Fabrication for Implantable Devices

Scope and specification options. Every figure is confirmed for your program in the quotation.

80/20
AuSn standard ratio
Test first
Each step tried on your own polymer
Ti/Au · Pt
Electrode metals
4 to 8 in
Carrier wafer diameters
Metal on polyimide
AuSn on UBM pads
Lift-off patterning
Glass through-vias
Electrode arrays
Glass bonding
Specification

Typical ranges

Typical windows; the quotation states the values for your stack.

ParameterTypicalNote
SubstratesPolyimide on glass or silicon carriers; polyimide film; borosilicate glass; siliconPolymer coated by you, or specified with us
MetalsTi/Au, Ti/Pt/Au, Pt; AuSn 80/20Ti adhesion layers rather than Cr for electrodes
AuSnAu/Sn multilayer, shipped as depositedThickness set by pad size and standoff
Substrate temperatureTypically stays below about 150 °C during AuSn depositionConfirmed per program for your polymer
Pad sizeAuSn pads from about 20 µm across by lift-offDepends on AuSn thickness; smaller features reviewed per layout
Wet stepsResist, strip and clean chemistry selected for your polymerSet up on process test wafers
Carrier wafers4 to 8 inch; ASIC wafer steps up to 12 inchFilm carriers per format
InspectionOptical inspection per wafer with photos; film thickness from a witness coupon in the same runOther measurements quoted separately
How a program runs

From stack review to qualified wafers

The first order is quoted as one program: trials on process test wafers, the photomasks, and the steps on your device wafers.

Process flow
01Stack review02Process test wafers03Confirm04First wafer05Deliver
  1. 01Stack reviewPolymer, cure, metals, layout, and thermal and chemical limits.
  2. 02Process test wafersResist, development and strip trialed on wafers with your polymer.
  3. 03ConfirmThicknesses, pad sizes and alignment confirmed in writing.
  4. 04First waferOne device wafer through development and inspected before the rest.
  5. 05DeliverInspection report with photos; repeat lots on the qualified flow.
What to send

For an implantable device quotation

ItemWhat helps
SubstrateCarrier material, diameter and thickness; polymer type and thickness
LimitsCure condition, maximum temperature, and chemistries the polymer must not see
StackMetals and pad finish on each layer; bonding method for the chips
LayoutGDS or DXF with a layer map and alignment marks
WafersDevice wafers, and process test wafers carrying the same polymer
ScheduleQuantity, target date, and the repeat lots you expect
Direct answers

Questions engineers ask before ordering

Can AuSn be deposited on polyimide?

Yes. AuSn is patterned by lift-off on UBM pads over polyimide. The resist, strip and clean steps are set up first on process test wafers carrying the same polyimide.

Does the AuSn need a reflow before shipment?

No. The Au/Sn multilayer is shipped as deposited and alloys during your bonding reflow.

Why process test wafers first?

Depending on its cure, a polyimide can react to developers, strippers and ultrasonic cleaning. Trial steps on wafers with your own polymer show what the film tolerates before a device wafer is committed.

Can you make glass feedthrough parts?

Through-glass vias are part of our TGV work. Feedthrough design, via fill and any sealing step are reviewed per program, and leak or hermeticity testing is agreed separately.

Do you handle biocompatibility or regulatory testing?

Biocompatibility, sterilization and regulatory testing stay with your program. We fabricate to the agreed process and film specifications.

Can you also prepare the ASIC wafers?

Yes. UBM and bumps on your ASIC wafers are covered on post-processing for foundry wafers.

Related service

PI Film & SUS Sensor Fab: the process most often combined with this work, run in the same program.

View page →

Start your project.
Initial response typically within one business day.

Share your process requirements, substrate, and production volume. A Nanosystems JP Inc. engineer gives an initial response, typically within one business day. A written quotation typically follows within 7-10 business days after we receive the required information and complete any prerequisite NDA.

To speed up technical review, please include:
substrate type & size  ·  target process  ·  quantity  ·  timeline  ·  design files if available (not required for first review)

sales@nanosystemsjp.co.jp · +81-3-5288-5569 · NDA available · All inquiries handled confidentially

Ready to discuss this process?
Initial engineering response typically within one business day. NDA available on request.
Request a Quote →
Services & Industries
Capabilities Overview
Substrates
Substrate & WafersSi, SiC, GaN, glass, sapphire Fused Silica WafersQuartz · borosilicate · low CTE Glass ProcessingDrilling, etching, polishing PI Film & SUS Sensor FabRoll-to-roll · sensor patterning
Front-End
Mask FabricationGDS to chrome mask, DRC PhotolithographyE-beam 20 nm to 500 × 600 mm NanoimprintingUV & thermal NIL Thin Film DepositionPVD, CVD, ALD, MBE ALD CoatingConformal oxides, nitrides PECVD DielectricsSiO₂, SiN, SiON, a-Si TFT & BackplaneIGZO · Glass · Display Lift-OffMetal pattern · shadow mask ElectroplatingCu TSV fill, DPC, LIGA Electroforming & LIGANi shims, meshes, microstructures EtchingICP-RIE, DRIE >50:1 ICP-RIE EtchingSi, oxide, III-V, SiC, quartz MEMS FoundrySensors, actuators, microfluidics Microchannel CoolingEtched, bonded, heater test chips Thermal Test ChipsHeater dies, multi-zone, RTD Temperature SensorsPt/NiCr RTDs, thermocouples AnnealingN₂ / H₂ / vacuum / RTA Ion ImplantationB / P / As / Al / N implant CMP & GrindingCu CMP, 50 µm thinning Wafer ThinningTo 50 µm on carriers Backside MetallizationTi/Ni/Ag, Ti/Ni/Au, Ti/Cu Patterned Test WafersCustom CMP and process evaluation wafers Daisy-Chain Test DiesDummy dies, chains, bump options DicingBlade, stealth laser Stealth & Laser Dicing300 mm Si and glass, SDBG Wafer CleaningRCA, plasma, megasonic Cleaning ChemistryPiranha, SC-1, SC-2, RCA
Advanced Packaging
Wafer BondingHybrid, eutectic, fusion Anodic BondingGlass to silicon, cavities MEMS Cap WafersCavities, ports, seal lands, bonded TSV FabricationHigh AR, Cu fill InterposersSi and glass, TSV/TGV + RDL TSV RevealBackgrind → etch → CMP TGV FabricationThrough-glass via Glass TGV CouponsHole-only to routed prototypes RDL FabricationBCB / PBO / PI + damascene Packaging & AssemblyWire bond, flip-chip Flip-Chip BondingTC, reflow, AuSn, underfill 3D / 2.5D PackagingTSV + RDL + UBM + C4 AuSn BumpPVD lift-off, fluxless Laser SubmountsSi/AlN submounts, optical benches Indium BumpEvap lift-off · cryo/quantum UBM DepositionTi/Pt/Au · adhesion-barrier-Au Foundry Wafer Post-ProcessingUBM, bumps, RDL on your wafers Cu Pillar & SnAg BumpingPillars with SnAg caps, SnAg bumps Gold BumpEvap & plated · Au-Au TC AuGe / AuSi361/363 °C eutectic die attach High-Pb Bumps95Pb5Sn · hi-rel C4 SLID / TLPCu/Sn · Au/In · Ag/In Al-Ge Sealing424 °C · CMOS-friendly MEMS Ohmic ContactsGaAs · GaN · RTA + TLM SiC ProcessingThinning, films, contacts, dicing GaN & III-VGaN, GaAs, InP processing Cryo / UHV MetalAuSn · Ti/Pd/Au · rings Optical AccessWindows · meshes · holes Vapor CellsDRIE + bond · unfilled TFOI WafersQuartz-on-Si · LNOI Biochip & MicrofluidicsGlass 500 × 600 mm, NIL Neural InterfacesMEA · probes · flexible arrays SiPho PackagingTSV · RDL · UBM · C4 for PIC Photonic DevicesSiN/SOI waveguides, gratings
Industries
AI & HPC PackagingCoWoS-style, 2.5D / 3D Silicon PhotonicsSOI · AuSn · TSV interposer AutomotiveMEMS sensors, SiC power Life SciencesLab-on-chip, biosensors Implantable DevicesMetal and AuSn on polyimide Detectors & InstrumentsDummy wafers, interposers RF & mmWaveHR-Si TSV · glass TGV Power DevicesBackside steps · SiC contacts All Industries → Request a Quote →